Optical constants of Cu-Zn (Copper-zinc alloy, Brass)
Querry 1985: n,k 0.21–55.6 µm; 70% Cu 30% Zn
Wavelength:
µm
(0.2100 – 55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
70% Cu, 30% Zn.
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)