RefractiveIndex.INFO

Refractive index database


nk database   |   n2 database   |   about

Shelf

Book

Page

Optical constants of CsPbI3 (Cesium lead triiodide)
Aftenieva et al. 2023: n,k 0.300–1.20 µm

Wavelength: µm
 (0.3000–1.2000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Cesium lead triiodide (CsPbI3) perovskite nanocrystals

References

O. Aftenieva, J. Brunner, M. Adnan, S. Sarkar, T. A. F. König. Directional amplified photoluminescence through large-area Perovskite-based metasurfaces. ACS Nano 2399–2410 (2023) (See Supporting information. Numerical data kindly provided by Tobias König)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Cesium lead triiodide

About Perovskite