Optical constants of CsPb(Br,Cl)3 (Cesium lead tribromide - Cesium lead trichloride)
Ermolaev et al. 2023: Br-1.3, Cl-1.7; n,k(e) 0.455–0.500 µm

Wavelength: µm
 (0.455–0.500)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions & Spec sheet

n_is_absolute: true
wavelength_is_vacuum: true

Comments

CsPbBr1.3Cl1.7 monocrystal. Extraordinary ray (e).

References

G. Ermolaev, A. P. Pushkarev, A. Zhizhchenko, A. A. Kuchmizhak, I. Iorsh, I. Kruglov, A. Mazitov, A. Ishteev, K. Konstantinova, D. Saranin, A. Slavich, D. Stosic, E. S. Zhukova, G. Tselikov, A. D. Carlo, A. Arsenin, K. S. Novoselov, S. V. Makarov, V. S. Volkov. Giant and tunable excitonic optical anisotropy in single-crystal halide perovskites, Nano Lett. XXX, XXX (2023) (Numerical data kindly provided by Georgy Ermolaev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Perovskite

External links