Optical constants of Cs2AgBiBr6 (Cesium silver bismuth bromide, CABB)
Jöbsis et al. 2021: n,k 0.300–1.70 µm
Wavelength:
µm
(3.000E-01–1.698E+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Cs2AgBiBr6 thin films of 100 nm at room temperature
References
H. J. Jöbsis, V. M. Caselli, S. H. C. Askes, E. C. Garnett, T. J. Savenije, F. T. Rabouw, E. M. Hutter. Recombination and localization: Unfolding the pathways behind conductivity losses in Cs2AgBiBr6 thin films. Appl. Phys. Lett. 119, 131908 (2021) (Numerical data kindly provided by Huygen Jöbsis)
Data
Additional information
About Cesium silver bismuth bromide
Other names and variations:
- Cs2AgBiBr6
- CABB