Optical constants of Bombyx mori (silkworm) silk
Perotto et al. 2017: Crystallized fibroin film; n 0.3–1.7 µm

Wavelength: µm
 (0.3–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.5303+0.0066λ^{-2}+1.1\text{×}10^{-4}λ^{-4}$$

Comments

Uncrystallized Bombyx mori (silkworm) fibroin film

References

G. Perotto, Y. Zhang, D. Naskar, N. Patel, D. L. Kaplan, S. C. Kundu, F. G. Omenetto. The optical properties of regenerated silk fibroin films obtained from different sources. Appl. Phys. Lett. 111, 103702 (2017)