Optical constants of Bombyx mori (silkworm) silk
Bucciarelli et al. 2018: Photocrosslinkable sericin film, crosslinked; n 0.4-1.5 µm
Wavelength:
µm
(0.4 – 1.5)
Derived optical constants
logX
logY
eV
Dispersion formula
$$n=1.524+6\text{×}10^{-3}λ^{-2}+4\text{×}10^{-4}λ^{-4}$$Comments
Photocrosslinkable sericin film. Formed using formic acid. Crosslinked.
References