Optical constants of AlSb-GaSb (Aluminium gallium antimonide, AlGaSb)
Ferrini et al. 1998: n,k 0.207-2.480 µm; 50% Al
Wavelength:
µm
(0.207 – 2.480)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
AlxGa1−xSb, x = 0.5. Thin film grown by molecular beam epitaxy on a GaSb substrate.
References
R. Ferrini, M. Patrini, and S. Franchi. Optical functions from 0.02 to 6 eV of AlxGa1−xSb/GaSb epitaxial layers, J. Appl Phys. 84, 4517-4524 (1998)