Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Perner et al. 2023: n 2.0–7.1 µm; 0% Al
Wavelength:
µm
(2–7.1)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{9.705183027405873λ^2}{λ^2-0.38586135365339097^2}$$Conditions
temperature: 295
Comments
Pure GaAs (interpolation for other alloy ratios possible). Relative standard uncertainty ≤3.3×10-4 over whole range. Optical measurements at 2.21 mbar and 22 °C.
References
L. W. Perner, G.-W. Truong, D. Follman, M. Prinz, G. Winkler, S. Puchegger, G. D. Cole, O. H. Heckl. Simultaneous measurement of mid-infrared refractive indices in thin-film heterostructures: Methodology and results for GaAs/AlGaAs. Phys. Rev. Res. 5, 033048 (2023) (Data kindly provided by the authors)