Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Papatryfonos et al. 2021: n,k 0.260-1.88 µm; 34.2% Al
Wavelength:
µm
(0.26049 – 1.87868)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
AlxGa1-xAs; x = 0.342
References
K. Papatryfonos, T. Angelova, A. Brimont, B. Reid, S. Guldin, P. R. Smith, M. Tang, K. Li, A. J. Seeds, H. Liu, D. R. Selviah. Refractive indices of MBE-grown AlxGa1-xAs ternary alloys in the transparent wavelength region, AIP Adv. 11, 025327 (2021) (Numerical data kindly provided by Konstantinos Papatryfonos)
Data
INFO
Aluminium gallium arsenide, AlGaAs
Other name
- Aluminum gallium arsenide