Optical constants of AlAs-GaAs (Aluminium gallium arsenide, AlGaAs)
Papatryfonos et al. 2021: n,k 0.260-1.88 µm; 0% Al
Wavelength:
µm
(0.26049 – 1.87868)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
AlxGa1-xAs; x = 0 (GaAs)
References
K. Papatryfonos, T. Angelova, A. Brimont, B. Reid, S. Guldin, P. R. Smith, M. Tang, K. Li, A. J. Seeds, H. Liu, D. R. Selviah. Refractive indices of MBE-grown AlxGa1-xAs ternary alloys in the transparent wavelength region, AIP Adv. 11, 025327 (2021) (Numerical data kindly provided by Konstantinos Papatryfonos)
Data
INFO
Aluminium gallium arsenide, AlGaAs
Other name
- Aluminum gallium arsenide