Optical constants of AgGaS2-AgInS2
Kato et al. 2021: n(o) 0.565–10.6 µm

Wavelength: µm
 (0.565–10.6)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=11.15176+\frac{0.23052}{λ^2-0.07319}+\frac{11918.07}{λ^2-2224.38}$$

Comments

AgGa0.86In0.14S2. Ordinary ray (o). Room temperature.

References

K. Kato, S. Banerjee, N. Uemura. Phase-matching properties of AgGa0.86In0.14S2 for three-wave interactions in the 0.615−10.5910 μm spectral range, Opt. Mater. Express, 11, 2800–2805 (2021)