Optical constants of AgGaS2-AgInS2
Kato et al. 2021: n(e) 0.565–10.6 µm
Wavelength:
µm
(0.565 – 10.6)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=10.62054+\frac{0.22283}{λ^2-0.09609}+\frac{10591.78}{λ^2-2084.70}$$Comments
AgGa0.86In0.14S2. Extraordinary ray (e). Room temperature.
References
K. Kato, S. Banerjee, N. Uemura. Phase-matching properties of AgGa0.86In0.14S2 for three-wave interactions in the 0.615−10.5910 μm spectral range, Opt. Mater. Express, 11, 2800–2805 (2021)