RefractiveIndex.INFO

Refractive index database


Shelf

Book

Page

Optical constants of 5PCH (4-trans-pentylcyclohexylcyanobenzene)
Wu et al. 1993: n(e) 0.4–0.8 µm; 53.4 °C

Wavelength: µm
 (0.4 – 0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=0.4429+\frac{1.6101}{25.0000-λ^{-2}}+\frac{0.9606}{18.1077-λ^{-2}}$$

Conditions & Spec sheet

temperature: 53.4 °C

Comments

53.4 °C. Extraordinary ray (e).

References

S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals, Opt. Eng. 32, 1775-1780 (1993)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Liquid crystals

Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.

External links