Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Wu et al. 1993: n(o) 0.4–0.8 µm; 34.8 °C
Wavelength:
µm
(0.4–0.8)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n-1=0.4165+\frac{1.4574}{22.6757-λ^{-2}}+\frac{0.5824}{12.5748-λ^{-2}}$$Conditions
temperature: 307.95 optical_component: o
Notes
34.8 °C. Ordinary optical constants (o).
References
S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)