Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Wu et al. 1993: n(e) 0.4–0.8 µm; 25.1 °C
Wavelength:
µm
(0.4–0.8)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n-1=0.4552+\frac{2.3250}{22.6757-λ^{-2}}+\frac{1.3970}{12.5748-λ^{-2}}$$Conditions
temperature: 298.25 optical_component: e
Notes
25.1 °C. Extraordinary optical constants (e).
References
S. T. Wu, C. Wu, W. Warenghem, M. Ismaili. Refractive index dispersions of liquid crystals. Opt. Eng. 32, 1775-1780 (1993)