Optical constants of 5CB (4-pentyl-4'-cyanobiphenyl)
Tkachenko et al. 2006: n(o) 0.532-1.7 µm
Wavelength:
µm
(0.532 – 1.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.50849+0.00774λ^{-2}+0.00040λ^{-4}$$Comments
Ordinary ray (o).
References
V. Tkachenko, G. Abbate, A. Marino, F. Vita, M. Giocondo, A. Mazzulla, F. Ciuchi, L. De Stefano. Nematic liquid crystal optical dispersion in the visible-near infrared range, Mol. Cryst. Liq. Cryst. 454, 263/[665]-271/[673], 2006