Optical constants of C3H7OH (Propanol)
Wang et al. 2018: iso-propanol, 70 °C; n,k 1.66–19.1 µm
Wavelength:
µm
(1.660 – 19.06)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 70.0 °C
Comments
Isopropanol, 70 °C.
References
C. C. Wang, J. Y. Tan, C. Y. Jing, L. H. Liu. Temperature-dependent optical constants of liquid isopropanol, n-butanol and n-decane, Appl. Opt. 57, 3303-3311 (2018) (Numerical data kindly provided by Chengchao Wang)