Optical constants of (C8H8)n (Polystyrene, PS)
Myers et al. 2018: n,k 1.28–25.0 µm
Wavelength:
µm
(1.28246E+00 – 2.50194E+01)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 26 °C
Comments
Isopropanol. 26 °C.
References
T. L. Myers, R. G. Tonkyn, T. O. Danby, M. S. Taubman, B. E. Bernacki, J. C. Birnbaum, S. W. Sharpe, T. J. Johnson. Accurate measurement of the optical constants n and k for a series of 57 inorganic and organic liquids for optical modeling and detection, Appl. Spectrosc. 72, 535-550 (2018) (see Supplemental Material for numerical data)