Optical constants of (C2H6OSi)n (Polydimethylsiloxane, PDMS)
Querry 1987: SF-96 fluid; n,k 0.82–2.5 µm
Wavelength:
µm
(0.8190 – 2.4990)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
SF-96 polydimethylsiloxane fluid
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)
Data
INFO
Polydimethylsiloxane, (C2H6OSi)n
Other names
- PDMS
- Poly(dimethylsiloxane)
- Dimethicone
- Dimethylpolysiloxane
Food additive code
- E900
Trademarks
- SF-96 (Momentive)
- RTV 615 (Momentive)
- Sylgard 184 (Dow)