Optical constants of (C5H8O2)n (Poly(methyl methacrylate), PMMA)
Tsuda et al. 2018: Lorentz-Drude model; n,k 2.50–18.2 µm

Wavelength: µm
 (2.50 – 18.18)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

MicroChem PMMA resist with a molecular weight of 950,000; Baked at 100 ℃ for 10 min on a hot plate; Lorentz-Drude model parameters provided in Table 1 of manuscript.

References

S. Tsuda, S. Yamaguchi, Y. Kanamori, and H. Yugami. Spectral and angular shaping of infrared radiation in a polymer resonator with molecular vibrational modes, Opt. Express 26, 6899-6915 (2018)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Poly(methyl methacrylate), (C5H8O2)n

Other names

  • Poly(methyl methacrylate)
  • PMMA
  • Acrylic glass

Trademarks

  • Plexiglas
  • Vitroflex
  • Limacryl
  • R-Cast
  • Per-Clax
  • Perspex
  • Plazcryl
  • Acrylex
  • Acrylite
  • Acrylplast
  • Altuglas
  • Polycast
  • Oroglass
  • Lucite

External links