Optical constants of (C5H8O2)n (Poly(methyl methacrylate), PMMA)
Tsuda et al. 2018: n 0.6–1.0 µm
Wavelength:
µm
(0.6 – 1)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.470+0.008354λ^{-2}-0.0008309λ^{-4}$$Comments
MicroChem PMMA resist with a molecular weight of 950,000; Baked at 100 ℃ for 10 min on a hot plate.
References
S. Tsuda, S. Yamaguchi, Y. Kanamori, and H. Yugami. Spectral and angular shaping of infrared radiation in a polymer resonator with molecular vibrational modes, Opt. Express 26, 6899-6915 (2018)