Optical constants of CH3OH (Methanol)
Chang et al. 2024: n 0.4–2.0 µm

Wavelength: µm
 (0.4–2)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.7316λ^2}{λ^2-0.119^2}$$

Conditions & Spec sheet

n_is_absolute: false
wavelength_is_vacuum: false
temperature: 295

Comments

21.5–22.0 °C

References

H.-J. Chang, N. Munera, C. Lopez-Zelaya, D. Banerjee, G. Beadie, E. W. Van Stryland, D. J. Hagan. Refractive index measurements of liquids from 0.5 to 2 µm using Rayleigh interferometry, Opt. Mater. Express 14, 1253–1267 (2024)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Methanol, CH4O

Methanol (CH4O), also known as wood alcohol, is a clear, colorless liquid with a slightly sweet odor. It is the simplest alcohol and is used as an antifreeze, solvent, fuel, and as a feedstock for producing various chemicals. Methanol is flammable and is toxic when ingested, inhaled, or absorbed through the skin. It can cause blindness if ingested. In the field of optics, methanol is often utilized as a solvent in various spectroscopic studies due to its ability to dissolve a wide range of organic compounds.

Chemical formula

CH3OH or MeOH

Other names

  • Hydroxymethane
  • Methyl alcohol
  • Methyl hydrate
  • Methyl hydroxide
  • Methylic alcohol
  • Methylol
  • Wood alcohol

External links