Optical constants of C7H17O3P (Diisopropyl methylphosphonate, DIMP)
Querry 1987: Near-infrared; n,k 0.81-2.5 µm
Wavelength:
µm
(0.8140 – 2.4990)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)