Optical constants of Zr (Zirconium)
Palm et al. 2018: n,k 0.226–1.68 µm

Wavelength: µm
 (0.226076263 – 1.684528687)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Zirconium, Room temperature, 200 nm thin film, electron beam evaporated, vacuum annealed 2 hr 350 °C.

References

K. J. Palm, J. B. Murray, T. C. Narayan, J. N. Munday. Dynamic optical properties of metal hydrides, ACS Photonics 5, 4677-4686 (2018)
(Numerical data kindly provided by Kevin Palm)