Optical constants of ZnSe (Zinc selenide)
Querry 1987: n,k 0.500-21.7 µm
Wavelength:
µm
(0.5000 – 21.7391)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)