Optical constants of YVO4 (Yttrium orthovanadate)
Shi et al. 2001: n(o) 0.48-1.34 µm; 20 °C
Wavelength:
µm
(0.48 – 1.34)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.778790+\frac{0.070479}{λ^2-0.045731}-0.009701λ^{2}$$Conditions & Spec sheet
temperature: 20 °C
Comments
Ordinary ray (o), 20 °C.
References
H. S. Shi, G. Zhang and H. Y. Shen. Measurement of principal refractive indices and the thermal refractive index coefficients of yttrium vanadate, J. Synthetic Cryst. 30, 85-88 (2001)
Data
INFO
Yttrium orthovanadate, YVO4
Other name
- Yttrium vanadate