Optical constants of YVO4 (Yttrium orthovanadate)
Shi et al. 2001: n(e) 0.48–1.34 µm; 140 °C
Wavelength:
µm
(0.48 – 1.34)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=4.613554+\frac{0.017202}{λ^2-0.055974}-0.014652λ^{2}$$Conditions & Spec sheet
temperature: 140 °C
Comments
Extraordinary ray (e), 140 °C.
References
H. S. Shi, G. Zhang and H. Y. Shen. Measurement of principal refractive indices and the thermal refractive index coefficients of yttrium vanadate, J. Synthetic Cryst. 30, 85-88 (2001)
Data
INFO
Yttrium orthovanadate, YVO4