Optical constants of WSe2 (Tungsten diselenide)
Gu et al. 2019: 2-layer (2L) film; n,k 0.193-1.69 µm
Wavelength:
µm
(0.1930 – 1.6900)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 2L substrate: sapphire
Comments
2-layer, 2L
References
H. Gu, B. Song, M. Fang, Y. Hong, X. Chen, H. Jiang, W. Ren, and S. Liu, Layer-dependent dielectric and optical properties of centimeter-scale 2D WSe2: evolution from a single layer to few layers. Nanoscale 11, 22762-22771 (2019) (Numerical data kindly provided by Baokun Song)