Optical constants of WS2 (Tungsten disulfide)
Jung et al. 2019: monolayer film; n,k 0.38–0.89 µm

Wavelength: µm
 (0.38135–0.89352)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 1L
substrate: Al2O3

Comments

CVD-grown monolayer; Room temperature

References

G.-H. Jung, S. Yoo, Q-H. Park. Measuring the optical permittivity of two-dimensional materials without a priori knowledge of electronic transitions. Nanophotonics 8, 263-270 (2019) - see Supplementary materials

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tungsten disulfide

Tungsten disulfide (WS2) is a layered transition metal dichalcogenide that possesses distinct properties based on its structural morphology. In its three-dimensional bulk form, WS2 has indirect bandgap semiconducting properties, which contrasts its behavior when isolated to a monolayer or few-layer forms. When exfoliated to these thin layers, WS2 undergoes a transition to a direct bandgap semiconductor, making it intriguing for potential applications in electronics, optoelectronics, and photonics. This material's unique hexagonal structure gives it excellent lubrication capabilities, often preferred in environments with high pressures and temperatures. Furthermore, research continues into its promise in nanoelectronic devices, spintronic applications, and as a component in heterostructures with other two-dimensional materials.

Other names and variations

  • WS2

Links