Optical constants of WS2 (Tungsten disulfide)
Hsu et al. 2019: 3-layer (3L) film; n,k 0.40–0.85 µm

Wavelength: µm
 (0.39697 – 0.85023)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions & Spec sheet

n_absolute: true
wavelength_vacuum: true
film_thickness: 3L

Comments

3-layer (3L)

References

C. Hsu, R. Frisenda, R. Schmidt, A. Arora, S. M. de Vasconcellos, R. Bratschitsch, H. S. J. van der Zant, A. Castellanos-Gomez. Thickness-dependent refractive index of 1L, 2L, and 3L MoS2, MoSe2, WS2, and WSe2, Adv. Optical Mater. 7, 1900239 (2019) (Numerical data kindly provided by Andres Castellanos-Gomez)