Optical constants of Sn (Tin)
Golovashkin and Motulevich 1964: n,k 0.73–12 µm; 293 K
Wavelength:
µm
(0.73 – 12)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 293 K
Comments
293 K (19.85 °C)
References
A. I. Golovashkin and G. P. Motulevich. Optical and electrical properties of tin, Sov. Phys. JETP 19, 310-317 (1964)