Optical constants of SiC (Silicon carbide)
Wang et al. 2013: 6H-SiC; n(o) 0.436–2.33 µm
Wavelength:
µm
(0.4358 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=6.57232+\frac{0.1401}{λ^2-0.03178}-0.02153λ^{2}$$Comments
6H-SiC (hexagonal crystal structure); Ordinary ray (o)
References
S. Wang, M. Zhan, G. Wang, H. Xuan, W. Zhang, C. Liu, C. Xu, Y. Liu, Z. Wei, X. Chen. 4H-SiC: A new nonlinear material for midinfrared lasers, Laser Photonics Rev. 7, 831–838 (2013)