Optical constants of Si (Silicon)
Šik et al. 1998: n,k 0.29–0.62 µm; 250 °C
Wavelength:
µm
(0.2883 – 0.6199)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 250 °C
Comments
Temperature: 250 °C (523 K).
References
J. Šik, J. Hora, J. Humlı́ček. Optical functions of silicon at high temperatures, J. Appl. Phys. 84, 6291–6298 (1998)
Data
INFO
Silicon, Si
Other names for Polysilicon
- Polycrystalline silicon, "poly"
- semicrystalline silicon