Optical constants of Si (Silicon)
Green 2008: n,k 0.25–1.45 µm
Wavelength:
µm
(2.5000e-01 – 1.4500e+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 300 K
Comments
Combination of data sets enforcing KK consistency. 300 K (27 °C). k is for band-to-band absorption.
References
M. A. Green. Self-consistent optical parameters of intrinsic silicon at 300K including temperature coefficients, Sol. Energ. Mat. Sol. Cells 92, 1305–1310 (2008)
Data
INFO
Silicon, Si
Other names for Polysilicon
- Polycrystalline silicon, "poly"
- semicrystalline silicon