Optical constants of Si (Silicon)
Green and Keevers 1995: n 0.25–1.45 µm, k 0.25–1.00 µm
Wavelength:
µm
(0.25 – 1.45)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
300 K (27 °C)
References
M. A. Green and M. J. Keevers. Optical properties of intrinsic silicon at 300 K, Progress in photovoltaics 3, 189-192 (1995)
Data
INFO
Silicon, Si
Other names for Polysilicon
- Polycrystalline silicon, "poly"
- semicrystalline silicon