Optical constants of Si (Silicon)
Daub 1995: k 0.94–1.42 µm
Wavelength:
µm
(9.4100e-01 – 1.4210e+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 295 K
Comments
Band-to-band absorption coefficient. Temperature: 295 K.
References
E. Daub. Photolumineszenz von Silizium Ph.D. dissertation, Dept. Phys., University of Karlsruhe, Karlsruhe, Germany, 1995 (as cited in C. Schinke, D. Hinken, J. Schmidt, K. Bothe, R. Brendel. Modeling the spectral luminescence emission of silicon solar cells and wafers, IEEE J. Photovolt. 3, 1038-1052 (2013))