Optical constants of RbTiOPO4 (Rubidium titanyl phosphate, RTP)
Carvajal et al. 2007: n(β) 0.4–1.5 µm
Wavelength:
µm
(0.4 – 1.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.0360+\frac{1.0883λ^{2}}{λ^2-0.0437}-0.0090λ^{2}$$Comments
nβ; 293 K (20 °C).
References
J. J. Carvajal, P. Segonds, A. Peña, J. Zaccaro, B. Boulanger, F. Díaz and M. Aguiló. Structural and optical properties of RbTiOPO4:Nb crystals , J. Phys.: Condens. Matter 19, 116214, 2007