Optical constants of Rb (Rubidium)
Whang et al. 1972: n,k 0.117-0.380 µm
Wavelength:
µm
(0.1165 – 0.3800)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
References
U. S. Whang, E. T. Arakawa, T. A. Callcott. Optical properties of Rb between 3.3 and 10.5 eV, Phys. Rev. B 5, 2118-2124 (1972)