Optical constants of Pd (Palladium)
Werner et al. 2009: n,k 0.0176–2.48 µm

Wavelength: µm
 (0.017586 – 2.479684)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions & Spec sheet

n_absolute: true
wavelength_vacuum: true

Comments

Experimental data: Derived from reflection electron energy-loss spectroscopy (REELS) spectra.

References

W. S. M. Werner, K. Glantschnig, C. Ambrosch-Draxl. Optical constants and inelastic electron-scattering data for 17 elemental metals, J. Phys Chem Ref. Data 38, 1013-1092 (2009)