Optical constants of Pb (Lead)
Golovashkin and Motulevich 1968: n,k 0.45–12 µm; 293 K
Wavelength:
µm
(0.45 – 12.0)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 293 K
Comments
293 K (19.85 °C)
References
A. I. Golovashkin and G. P. Motulevich. Optical properties of lead in the visible and infrared spectral ranges, Sov. Phys. JETP 26, 881-887 (1968)