Optical constants of Nb (Niobium)
Golovashkin et al. 1969: n,k 0.40–9.2 µm; 78 K
Wavelength:
µm
(0.40 – 9.20)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 78 K
Comments
78 K (-195.15 °C)
References
A. I. Golovashkin, I. E. Leksina, G. P. Motulevich and A. A. Shubin. The optical properties of niobium, Sov. Phys. JETP 29, 27-34 (1969)