Optical constants of NaCl (Sodium chloride)
Querry 1987: n,k 0.22-167 µm
Wavelength:
µm
(0.2200 – 166.6667)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)
Data
INFO
Sodium chloride, NaCl
Other names
- Salt
- Common salt
- Table salt
- Rock salt
Mineral
- Halite