Optical constants of Na (Sodium)
Ives and Briggs 1937: n,k 0.254–0.578 µm
Wavelength:
µm
(0.2536 – 0.5780)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
H. E. Ives and H. B. Briggs. The optical constants of sodium, J. Opt. Soc. Am. 27, 181-185 (1937)