Optical constants of MoS2 (Molybdenum disulfide)
Zotev et al. 2023: n,k(e) 0.36–1.0 µm
Wavelength:
µm
(0.3600–1.0000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_is_absolute: true wavelength_is_vacuum: true
Comments
Multilayer crystals. Out-of-plane (extraordinary ray, e). Room temperature.
References
P. G. Zotev, Y. Wang, D. Andres-Penares, T. Severs-Millard, S. Randerson, X. Hu, L. Sortino, C. Louca, M. Brotons-Gisbert, T. Huq, S. Vezzoli, R. Sapienza, T. F. Krauss, B. D. Gerardot, A. I. Tartakovskii. Van der Waals materials for applications in nanophotonics, Laser and Photonics Rev. 17, 2200957 (2023) (Numerical data kindly provided by Panaiot Zotev)