Optical constants of MoS2 (Molybdenum disulfide)
Jung et al. 2019: monolayer (1L) film; n,k 0.38–0.89 µm
Wavelength:
µm
(0.3813 – 0.89341)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 1L substrate: Al2O3
Comments
CVD-grown monolayer; Room temperature
References
G.-H. Jung, S. Yoo, Q-H. Park. Measuring the optical permittivity of two-dimensional materials without a priori knowledge of electronic transitions, Nanophotonics 8, 263-270 (2019) - see Supplementary materials