Optical constants of LuAl3(BO3)4 (Lutetium aluminium borate, LuAB)
Fang et al. 2013: n(e) 0.266–1.34 µm

Wavelength: µm
 (0.266 – 1.338)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=2.85939+\frac{0.01511}{λ^2-0.01429}-0.01116λ^{2}$$

Comments

25 °C. Extraordinary ray (e).

References

S. Fang, H. Liu, L. Huang, and N. Ye. Growth and optical properties of nonlinear LuAl3(BO3)4 crystals, Optics Express 21, 16415-16423 (2013)