Optical constants of Lu2O3 (Lutetium sesquioxide)
Kaminskii et al. 2008: n 0.365–2.325 µm
Wavelength:
µm
(0.365 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.61968+\frac{0.04131}{λ^2-0.0238}-0.00856λ^{2}$$Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
Room temperature
References
A. A. Kaminskii, M. Sh. Akchurin, P. Becker, K. Ueda, L. Bohatý, A. Shirakawa, M. Tokurakawa, K. Takaichi, H. Yagi, J. Dong. Mechanical and optical properties of Lu2O3 host-ceramics for Ln3+ lasants, Laser Phys. Lett. 5, 300-303, 2008