Optical constants of LiB3O5 (Lithium triborate, LBO)
Chen et al. 1989: n(α) 0.289-1.06 µm
Wavelength:
µm
(0.2894 – 1.064)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.45768+\frac{0.0098877}{λ^2-0.026095}-0.013847λ^{2}$$Comments
nα; Room temperature.
References
1) C Chen et al.. New nonlinear-optical crystal: LiB3O5, J Opt. Soc. Am. 6, 616-621 (1989)
2) F. Hanson and D. Dick. Blue parametric generation from temperature-tuned LiB3O5, Opt. Lett. 16, 205-207 (1991).
* Ref. 2 provides a dispersion formulas based on the experimental data from Ref. 1