Optical constants of Li (Lithium)
Mathewson and Myers 1971: n,k 0.326–1.77 µm; 298 K
Wavelength:
µm
(0.32627 – 1.77120)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 298 K
Comments
298 K (24.85 °C)
References
A. G. Mathewson and H. P. Myers. Absolute values of the optical constants of some pure metals, Phys. Scr. 4, 291-292 (1971)