Optical constants of K (Potassium)
Sutherland and Arakawa 1968: n 0.128–0.313 µm
Wavelength:
µm
(0.1280 – 0.3131)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
J. C. Sutherland and E. T. Arakawa. Optical properties of potassium for photons of energy 3.96 to 9.69 eV, J. Opt. Soc. Am. 58, 1080-1083 (1968)